Can a 1 kW Fiber Laser Cut Stainless Steel, Aluminium, Brass and Galvanized Sheet?
Can a 1 kW fiber laser cut stainless steel, and how thick can it go?
Yes. On the YM3015G a 1000 W fiber source cuts stainless steel up to 4 mm with nitrogen or clean compressed air, and this is the material most owners buy the machine for after carbon steel. Typical results with 99.95% nitrogen at 8-12 bar: around 8-12 m/min on 1 mm, 4-6 m/min on 2 mm, 2.5-3.5 m/min on 3 mm, and roughly 1.2-1.8 m/min on 4 mm 304. The edge comes out bright and oxide-free, which is why a nitrogen cut can go straight to welding or to a visible surface without pickling. Above 4 mm the 1 kW source runs out of energy density and you start seeing heavy dross, loss of verticality and a grey, oxidised face; a 5 mm 304 job on this machine is possible as a one-off but is not a production process. If your mix is mostly 5-8 mm stainless, specify 3 kW or more rather than fighting the limit every shift.
Can it cut aluminium sheet, or is aluminium too reflective for a laser?
It cuts aluminium up to 3 mm, with nitrogen at 12-15 bar and the focus set slightly below the surface. The reflectivity worry is real but it belongs to the CO2 era: at 10.6 microns aluminium reflects over 90% of the beam, while at the 1070-1080 nm wavelength of this fiber source the absorption is far higher and rises further once the melt starts. So the practical issue is not the beam bouncing back into the head, it is dross. Aluminium melts at 660 C, conducts heat away quickly and re-solidifies as a sticky, welded-on dross that is much harder to remove than steel dross. Expect to run slower than on stainless of the same thickness, to use high-pressure nitrogen rather than air for anything visible, and to keep the nozzle clean - a partially blocked nozzle on aluminium shows up immediately as dross on one side of the cut. Aluminium above 3 mm is 3-6 kW territory.
What about brass and copper - can a 1 kW laser cut those?
Brass is specified to 3 mm on this machine and is cut with high-pressure nitrogen at reduced speed; expect a darker, slightly rougher edge than stainless and some dross on the underside because zinc starts to vaporise in the cut zone. Copper is the honest limit. At room temperature copper reflects around 95% of a 1 micron beam and conducts heat about eight times better than steel, so the little energy that is absorbed is pulled away from the kerf before it can melt through. A 1 kW source will manage thin copper foil and decor parts but is not a production tool for 2-3 mm copper busbar or plate. Those jobs belong to 3-6 kW fiber lasers with 15 bar+ nitrogen, or to waterjet if the edge must be burr-free and oxide-free. Be equally realistic about thick brass: 4 mm and up needs more power, not more passes.
What changes in gas, focus and nozzle when I switch from carbon steel to stainless or aluminium?
Three things change together, and changing only one is the usual reason a material switch fails. Gas: carbon steel is cut with oxygen, which is an exothermic assist and leaves a thin oxide film; stainless, aluminium and brass need nitrogen (99.95% minimum, 99.999% for a mirror-bright edge) or clean dry air for non-visible parts, because oxygen on stainless burns chromium at the cut face and leaves a dark, weld-rejectable edge. Focus: on thin non-ferrous sheet set focus at or just above the top surface (0 to +0.5 mm), on 3-4 mm set it just below (-0.5 to -1.5 mm); carbon steel of the same thickness usually wants a more negative focus. Nozzle: single or double nozzle of 1.2-1.5 mm with 0.8-1.2 mm standoff, and pressure at the nozzle rather than at the regulator - a 12 bar setting that reads 6 bar at the head will dross on 3 mm stainless. Save each material as its own parameter set and never tweak a saved set on the fly.
Why does stainless steel come out with dross or a burnt, yellow edge?
Read the defect as a message. A hard, granular dross that will not flake off means the cut is running too fast or gas pressure is too low for the thickness - reduce speed in 5% steps, then raise pressure. A soft, bubbly dross with a wide kerf means too slow or too much power, so the melt pool overheats and re-welds. A yellow-brown or blue tint on a nitrogen cut almost always means gas purity or gas flow, not the laser: moisture or oxygen in the line, a leaking hose, or a regulator icing up. A cut that is clean on one side of a part and drossy on the other usually points at nozzle alignment or a partially blocked nozzle orifice rather than at parameters. And if the same program that ran clean last week now drosses everywhere, check the protective window and the focus lens before touching any parameter - a contaminated optic costs you 10-20% of effective power and no amount of speed tuning will recover it.
Can you laser cut galvanized or zinc-coated sheet, and what happens to the coating?
Yes, and it is common in steel structure work for secondary parts. Two things to plan for. First, zinc boils at 907 C, well below the steel melting point, so it vaporises explosively in the kerf, throwing spatter, producing a heavier dross and a rougher edge than bare steel, and generating zinc oxide fume. Run galvanized at reduced speed with air or nitrogen, keep good extraction and a clean filter, and expect to replace the protective window more often. Second, the coating is lost for roughly 0.5-1 mm back from each cut edge, so a galvanized part that will be exposed must have its cut edges touched up with a zinc-rich paint if you are working to ISO 1461 expectations for corrosion protection. Never cut PVC-coated or plastic-film sheet without checking what the film is made of - PVC releases hydrogen chloride and attacks the machine and the part; PE film is the safe choice, and bare sheet is safer still.
Can I cut mirror-finish stainless, and is there any risk to the laser head?
You can, and modern fiber sources include back-reflection protection, so a reflective workpiece will not normally destroy the source. The risk sits elsewhere: mirror-finish sheet reflects spatter back onto the nozzle and the protective window, so windows and nozzles wear noticeably faster, and the reflected light makes the cut harder to monitor. Use a larger nozzle with good standoff, a fresh protective window, high-purity nitrogen, and reduce power slightly at the entry pierce. Pierce off the part whenever the geometry allows, because the pierce is where most spatter is generated. For safety, treat the whole enclosure as a laser area: interlocked guards, no looking into the cutting zone, and 1064 nm-rated eyewear only for maintenance with the enclosure open. Also remember that mirror sheet shows every scratch, so handling and slat contact matter as much as the cut itself.
What can a 1 kW fiber laser not do, and what should I use instead?
Be clear about the boundary so you do not buy the wrong machine. On this 1000 W / 3000x1500 mm platform the practical envelope is carbon steel to 12 mm, stainless to 4 mm, aluminium and brass to 3 mm - inside that envelope it is fast and precise (±0.05 mm/m positioning, 80 m/min rapid). Outside it, the right answers are different processes: carbon steel 15-25 mm and long straight bevels go to plasma or oxy-fuel far more cheaply; stainless and aluminium above 5 mm need a 3-6 kW fiber laser to stay economic; thick copper and any job that cannot tolerate a heat-affected zone belong to waterjet; and high-volume perforated or louvre work at 1-2 mm is usually faster on a turret punch. A fabricator who cuts 80% carbon steel 1-6 mm plus some stainless and aluminium trim is exactly the profile this machine was built for - a shop that is 60% 10 mm plate should be looking at plasma first.
Technical Specifications of CNC Laser Cutting Machine
| Parameter | Value |
|---|---|
| Share | |
| Categories | Plate Cutting Machine |
| Brand | YOMI CNC Cutting&Welding Machinery |
| Product Specifications | YM3015G |
| Material | Thickness, Auxiliary gas |
| Carbon Steel | ≤12mm, Oxygen/air |
| Stainless Steel | ≤4mm, Nitrogen/air |
| Aluminium Alloy | ≤3mm, Nitrogen/air |
| Brass | ≤3mm, Nitrogen/air |
| Equipment model | YM3015G |
| Type of laser | Optical fiber laser |
| Laser working medium | Fiber |
| Laser wavelength | 1060-1080 mm |
| Rated output power | 1000W |
| Beam quality | <0.373mrad |
| X-Axis travel | 3000mm |
| Y-Axis travel | 1500mm |
| Z-Axis travel | 100mm |
| Effective cutting range | 3000×1500mm |
| Table axial positioning accuracy | ±0.05mm/m |
| Table Repeated positioning accuracy | ±0.02mm/m |
| Maximum no-load running speed | 80m/min |
| Power rating parameters | Three-phase AC 380V 50Hz |
| Power of equipment | 11 KW |
| Total power protection level | IP54 |
| Auxiliary Gas | Oxygen, Nitrogen, Compressed Air |
| Working life of fiber module | More than 100000 hours |
| Packed size | 4626*2460*1734 mm (L*W*H) |
| Gross weight | About 2500 kg |
Product Gallery







Applications
The CNC Laser Cutting Machine is widely applied in steel structure prefabricated buildings, bridge and infrastructure construction, shipbuilding and marine engineering, heavy machinery manufacturing, power plant and industrial facilities, and offshore wind power structures.
Learn more about the CNC Laser Cutting Machine:
https://www.steelstructurer.com/pid18378002/CNC-Laser-Cutting-Machine.htm
For more information about CNC Laser Cutting Machine and other steel structure intelligent equipment, contact YOMI CNC Cutting & Welding Machinery. Our team of experts is ready to help you find the best solution for your manufacturing needs.

- Full Name:
- YOMI WhatsAPP
- Tel:
+86 19053498672
- Email:
- sales@yomi-china.com
- WhatsApp:
- 8619053498672
- Address:
- Factory Adress: 9 Changjie Road, Ningjin,Dezhou, P.R.China